Minh hoạ Welding inspection

UT vs RT for Weld Inspection: Practical QC Welding & NDT Selection Guide

When preparing an ITP (Inspection and Test Plan) for structural steel or process piping, QC Welding & NDT Engineers frequently face a key choice: specify UT (Ultrasonic Testing) or RT (Radiographic Testing)? Choosing the wrong method can delay site schedules or miss critical planar defects such as Lack of Fusion or Cracks.

Quick Selection Rule: UT vs RT

  • Choose UT when: Wall thickness is ≥ 8–10 mm, joints are CJP T-joints/corner welds, radiation exclusion zones are impractical, or planar flaws must be detected reliably.
  • Choose RT when: Piping is thin-walled (< 8 mm) or small-bore where UT probe scanning is limited, or when permanent visual film/digital image records are required by the Client.

Technical Comparison Table

CriterionUT (Ultrasonic Testing)RT (Radiographic Testing)
Best Flaw SensitivityPlanar flaws (cracks, lack of fusion, lamination)Volumetric flaws (porosity, slag inclusions)
Effective ThicknessTypically ≥ 8 mm (PAUT can cover thinner walls)Thin pipes < 8 mm up to ~50 mm
Site Safety & ScheduleNo radiation hazard; parallel work allowedRequires radiation barricade & night-shift scheduling
Permanent RecordWritten report (PAUT/TOFD stores digital scan data)X-ray / Gamma film or digital radiograph

Related: Piping Hydrotest QC Checklist per ASME B31.3.